PPG announced a $44 million investment to upgrade five powder coating manufacturing facilities in the United States and Latin America.
The company expects the overall investment — $30 million for U.S. plants and $14 million for facilities in Latin America — to increase overall capacity, add production capabilities for bonded metallic powders, improve processing times with automated packaging and enhance capabilities to produce small, medium and large batches. Enhancements and expansions are already completed or under way at powder production facilities in Brazil, Ind.; Gainesville, Texas; Greensboro, N.C.; San Juan del Rio, Mexico; and Sumaré, Brazil. PPG expects to complete these projects by the fourth quarter of 2023.
Since 2019, PPG has focused on growing its powder coatings capacity and capabilities, making four strategic acquisitions and expanding production and service elements at seven sites across the globe. A key factor driving the rapid adoption of powder coatings is the growing interest in more sustainable solutions. Powder coatings are generally formulated without solvents that release volatile organic compounds (VOCs) and in the application line, these coatings can be reclaimed and reused.
“Focusing on powder coatings is a win-win for PPG and our customers as we are able to offer greater access to sustainably advantaged products,” said Marizeth Carvalho, PPG global director, powder coatings, Industrial Coatings. “Powder is the fastest growing coatings technology in the world and PPG’s goal is to lead that charge through innovation and production advancements.” PPG is a supplier of powder coatings to the automotive, general industrial, appliance, furniture and other key industries. It has 21 powder manufacturing plants, of which seven have bonding capabilities, a powder resin plant and an R&D development center.