Nano-Mechanical Properties and Topography of Thermosetting Acrylic Powder Coatings

January 2001

Vol. 73, No. 912

By D.C. Andrei, J.L. Keddie, J.N. Hay, B.J. Briscoe, D. Parsonage

Both nano-scratching and nano indentation techniques have been used to evaluate the me­chanical properties of the surface of acrylic coat­ings, with and without added pigment. The coat­ings were formed from thermosetting, acrylic pow­ders. Both types of coatings-clear and pig­mented-do not exhibit any significant differ­ences in their hardness with an increase in baking time from 7 to 15 min. According to the scratch­ing profiles, the deformation induced at the sur­face is virtually elastic. Introducing the pigment causes a slight increase in the elastic modulus but no significant variation in hardness.

In all coat­ings, the computed hardness and the elastic modu­lus values are higher near the surface (perhaps as a result of tip geometry effects), but these readily reach plateau values that are consistent with other work available in the literature. A long-range surface profiler, which provided two-dimensional and three-dimensional topographical maps of the coating surfaces, reveals undulations in the sur­face with a wavelength on the order of 2-4 mm.

Moreover, the topography of the pigmented coat­ing is significantly smoother than that of the clear coating in which shallow pits (about 100 µm in diameter) are randomly distributed at the surface. The nano-mechanical properties within these pits are similar to the bulk of the coating.

Terms of Use

By clicking "Okay," or by continuing to access the website, you agree to be bound by the Terms of Use. Please read the Terms carefully, as they form an agreement between you and the American Coatings Association.