Evaluation of Organic Coatings with Electrochemical Impedance Spectroscopy – Part 3 – Protocols for Testing Coatings with EIS

February 2005

By David Loveday, Pete Peterson, Bob Rodgers

In Parts 11 and 22 of this Series, we discussed the technology of applying electrochemical impedance spectroscopy (EIS} to organic coatings on a metallic substrate such as aircraft, marine, or industrial maintenance coatings. This article describes several experimental proto­cols to evaluate these coatings with EIS. These experimental protocols differ primarily in the process used to stress the coating and accelerate the degradation of the coating.

There is no standard recipe for an EIS-based evaluation program that is guaranteed to work for every coating in every environment. This may come in time and, indeed, a standard for EIS evaluation of coatings is under development at ASTM and ISO. 3 However, EIS can be employed in a variety of ways to evaluate virtually any coating.
It may be useful to think of EIS as a very sensitive detector that provides a snapshot of coating status.

However, a single EIS measurement of an organic coating tells you nothing. To measure coating lifetime or performance, the coating must be stressed to bring about its failure. By making periodic EIS measurements during the stress process, a rate of coating failure can be estimated and a series of coatings may be ranked.

Even though some publications discuss the determination of the time-to-failure of a coat­ing, this may be an unrealistic goal. There are too many variables that separate us from this “Holy Grail,” most of which are not related to EIS. A more achievable objective is to use EIS in an experimental program that results in a performance ranking of a series of coatings for use in a specific environment. The nature of the stress applied to the coating is, of course, very important in several as­pects. The experimental design to prompt the failure of the coating must (1) simulate the service environment the coating will encounter and (2) it must not change the failure mech­anism.4

To use EIS to evaluate a specific coating system, (1) place the coated sample in an envi­ronment designed to accelerate the degradation of the coating, (2) measure the EIS curves over time, and (3) identify an “index” that tracks coating quality. The index could be the Coatings Capacitance or the Pore Resistance, for example. The index can be very simple or more complex and we will look at several examples in this article. Unfortunately, all coatings do not fail in the same way, so there is no universal index for assessing coating quality with EIS.

This complex nature of coatings is no surprise to coatings scientists. A coating system may consist of the metal substrate, surface pretreatment, a primer, and one or more topcoats. Results can vary depending on types of coatings, thickness, number of layers, surface treat­ment, and the nature of the metal substrate.