Surface Mold Prevention with Chlorothalonil/ Disodium Octaborate Tetrahydrate Systems
February 2008
By Joseph W. Burley
A laboratory study has confirmed the merit of topically applied chlorothalonil and chlorothalonil/disodium octaborate tetrahydrate combination systems for the prevention of fungal growth on wood ( and gypsum drywall) substrates. This article describes the extension of this work to a field study performed on construction lumber under harsh climatic conditions (southern Florida), highly favorable to mold growth.
This more realistic study also confirmed the effectiveness of chlorothalonil-based systems in prevention of surface infestation by mold fungi. The practical application of these systems for mold prevention in new home construction is discussed.