AkzoNobel’s Marine Coatings business and Winning Shipping in China signed a strategic agreement which they say will help accelerate the maritime industry’s transition to lower carbon operations.

The two companies have been partners since 2016 and the expanded collaboration will involve AkzoNobel supplying a significant volume of International® coatings for a number of drydocking projects in 2026. Focused on six vessels, it will enhance the fleet’s operational efficiency and environmental performance.

“The outstanding performance of International has been fully validated in our existing fleet, delivering significant fuel savings and enhancing our market competitiveness,” says Yu Shan, general manager of Qingdao Winning International Ship Management Co., Ltd.

“We’re honored to continue and deepen our strategic cooperation,” added Rob Leslie, commercial director of AkzoNobel Marine and Protective Coatings in Greater China. “Winning Shipping’s unwavering pursuit of more efficient operations aligns perfectly with our philosophy of helping customers through sustainable innovation. We look forward to providing solid support for the long-term operational efficiency and sustainable development goals of its fleet.”