CoatingsTech Archives
Coating Solutions Enabling Advanced Automotive Technologies
January 2020
By Cynthia Challener
The automotive industry is undergoing a significant transformation. Conventional internal combustion engines (ICEs) are being replaced by batteries in electric vehicles (EVs), and drivers will ultimately become passengers in autonomous vehicles (AVs). Coatings have an important role to play in making these new technologies possible. Beyond their traditional jobs of protecting automobile components from corrosion, abrasion, and ultraviolet (UV) degradation and providing a unique and striking appearance, automotive coatings are already providing additional functionality.
This includes soft-touch and sound-dampening interior surfaces and self-healing and easy-to-clean exterior surfaces. Additional performance capabilities are being achieved on a continual basis, with some technologies adopted from other industrial applications and others developed specifically to meet the needs of the evolving automotive sector. The future of the automotive industry will be heavily dependent on electric and hybrid vehicles, as well as autonomous vehicles, according to Christopher M. Seubert, research engineer in the Paint and Coatings Research group at the Ford Research and Innovation Center.
“As we look at the current industry transformation, the focus is on CASE solutions connected, autonomous, shared, and electrified,” adds Peter Votruba-Drzal, global technical director for PPG. As companies explore connected and autonomous vehicles and new, alternative powertrains, coatings need to be adapted to meet these needs, asserts David Cranfill, BASF technical director for OEMs.