Pigments ll – Growing Demand for Specialty Effect Pigments
July 2004
By Cynthia Challener,
Like high-value organic pigments, specialty effect pigments find most applications in automotive coatings, although use of these high-value pigments is increasing in consumer goods and security applications. At the present, the market is growing at a healthy rate, but competition from offshore producers is expected to become an issue in the near future. Major suppliers of effect pigments are focusing on the development of novel technologies and products that differentiate themselves from the competition.
The global specialty effect pigment market is growing at approximately 7% per year and is estimated to be worth $1.287 billion in 2004, up from $ 1.065 billion in 2001, according to Mike Brown of the ChemQuest Group, Inc., a management consulting firm located in Cincinnati, OH. Mica pearlescent and aluminum flake pigments account for 94% of sales ( 50°/o and 44%, respectively). Mica pigments sales are growing at 8% per year and are estimated by ChemQuest to reach $649 million in 2004. Aluminum-based pigments are pegged at $562 million in 2004 with an annual growth rate of 4%. The remaining 6% of sales are attributed to other specialty effect pigments, particularly color shift pigments. Sales for this category are estimated to top $ 7 6 million in 2004 and are growing at a rapid 15% annually.