CoatingsTech Archives
Low VOC Carbamate Functional Coatings Compositions for Automotive Topcoats
July 2001
Vol. 73, No. 918
By Marvin L. Green
Polymers and oligomers having carbamate functional groups have been used in a variety of curable coating compositions. Carbamate functional polymers offer many advantages for automotive topcoats, such as outstanding resistance to environmental etching, scratching and marring, humidity, and UV exposure.
Hydrophobic carbamate oligomers suitable for crosslinking with standard amino resins were synthesized and formulated into stable one-pack automotive clearcoats with low volatile organic compound (VOC) and excellent physical properties.
Because of their unusually steep thermal viscosity curves, these oligomers are particularly adaptable to hot spray techniques that enable coatings in the 85-90% weight solids range to be applied with conventional electrostatic mini-bells.