Accelerated Corrosion Testing for Bisphenol-A Non-Intent Metal Packaging Resin
[…] development cycles. References Geueke, B. “France Bans BPA,” Food Packaging Forum (website), January 6, 2015, https://www. foodpackagingforum.org/news/france-bans-bpa (accessed July 22, 2020). Commission Regulation (EU) 2018,213 on the use of bisphenol […]