Factors Affecting Sealer Performance on Concrete
[…] to create the data and Ingrid Meier and Maria Nargiello for editorial assistance. References https://en.wikipedia.org/wiki/Concrete_sealer. Understanding Concrete Sealers and Chemicals, Seminar TH140, WoC2011. https://www.understanding-cement.com/hydration.html. https://www3.imperial.ac.uk/concretedurability/researchprojects/predictingmasstransport. Comparison of Waterborne and […]