Members Only Testing Accelerated Weathering Tests for Appropriate Weathering Chemistry: Ozone Filtered Xenon Arc
FTIR spectroscopy has been used to follow the weathering chemistry of a HALS and UVA free poly-ester/urethane and a HALS and UVA free acrylic/melamine clearcoat cured on silicon wafers and […]